Mechanical Properties Metric English Comments
Flexural Modulus 18.6 GPa
2700 ksi
1.3 mm/min; ASTM D790
Ovation Polymers Nemcon™ E PK DP104 Polyetheretherketone, Carbon Fiber Reinforced
Nemcon™ E PK DP104 is a carbon fiber reinforced polyetheretherketone, characterized by high strength, stiffness, consistent moldabiliity, and exceptional thermal resistance.All properties after 48h..
Flexural Modulus 18.6 GPa

@Temperature 23.9 °C
2700 ksi

@Temperature 75.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® S-860 Silicone Prepreg, 1581-112NPH E-Glass Reinforced
Nelcote® S-860 is a MIL-P-25518 type silicone resin with a good combination of electrical and high temperature properties. GMS4001 qualified specificationsKey Features and Benefits:500°F maximum s..
Flexural Modulus 18.6 GPa
2700 ksi
Lengthwise; ASTM D790
G-10 Fiberglass Epoxy Laminate Sheet
This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e..
Flexural Modulus 18.6 GPa
2700 ksi
Crosswise; ASTM D790
G-11 Fiberglass Epoxy Laminate Sheet
This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e..
Flexural Modulus 18.6 GPa
2700 ksi
ASTM D790
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Flexural Modulus 18.6 GPa
2700 ksi
ASTM D790
Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced
Carbon Fiber Reinforced
Flexural Modulus 18.6 GPa
2700 ksi
ASTM D790
Techmer ES HiFill® PEEK CF20 TL15 HF 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: High Flow and LubricatedInformation provided by TP Composi..
Flexural Modulus 18.6 GPa
2700 ksi
ASTM D790
Techmer ES Luriblend® PA6/6 CF30 TL12 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceTPCI# 6466101Inf..
Flexural Modulus 18.6 GPa
2700 ksi
GB/T 9341-2008
Sichuan Deyang Haton® hGR515 Polyphenylene Sulfide/PA Alloy
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD
Flexural Modulus 18.6 GPa
2700 ksi
ASTM D790
Techmer ES HiFill® PA4/6 CF40 IM HS 40% Carbon Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites..
Flexural Modulus 18.6 GPa
2700 ksi
ISO 178
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Dry
Information provided by Unitika Ltd.
Flexural Modulus 18.6 GPa
2700 ksi
45° stress angle
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..
Flexural Modulus 18.6 GPa
2700 ksi
ASTM D790
PolyOne Edgetek® PF-40CF/000 Polysulfone, Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 18.6 GPa
2700 ksi
ASTM D790
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..