G-11 Fiberglass Epoxy Laminate Sheet

Category Polymer , Thermoset , Epoxy , Filled/Reinforced Thermoset
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF G-11 Fiberglass Epoxy Laminate Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and electronic test equipment and electric rotor insulation. G-11 is difficult to cut or machine and may require special equipment. G-10 is slightly stronger while G-11 is a better insulator and can withstand higher temperatures. G-11 and similar fiberglass reinforced thermosets are sometimes known as garolite.Information provide by Boedeker Plastics.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hrs.; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 112
112
ASTM D785
Tensile Strength at Break 255 MPa
37000 psi
Crosswise; ASTM D638
296 MPa
43000 psi
Lengthwise; ASTM D638
Flexural Strength 483 MPa
70000 psi
Crosswise; ASTM D790
552 MPa
80000 psi
Lengthwise; ASTM D790
Flexural Modulus 18.6 GPa
2700 ksi
Crosswise; ASTM D790
20.7 GPa
3000 ksi
Lengthwise; ASTM D790
Compressive Strength 434 MPa
63000 psi
ASTM D695
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
Crosswise; ASTM D256
6.41 J/cm
12.0 ft-lb/in
Lengthwise; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 13.0 µm/m-°C

@Temperature 20.0 °C
7.20 µin/in-°F

@Temperature 68.0 °F
Lengthwise; ASTM D696
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Crosswise; ASTM D696
Thermal Conductivity 0.288 W/m-K
2.00 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 165 °C
329 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 4.5

@Frequency 1e+6 Hz
4.5

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 35.4 kV/mm
900 kV/in
Short Time; 1/8 inch; ASTM D149
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 sec
120 sec
ASTM D495