Techmer ES HiFill® PA4/6 CF40 IM HS 40% Carbon Filled (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 46
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA4/6 CF40 IM HS 40% Carbon Filled (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Water Absorption 1.7 %

@Time 86400 sec
1.7 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Thickness 3.17 mm
0.0012 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 207 MPa
30000 psi
ASTM D638
Elongation at Break 3.2 %
3.2 %
ASTM D638
Flexural Strength 345 MPa
50000 psi
ASTM D790
Flexural Modulus 18.6 GPa
2700 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm

@Thickness 3.17 mm
1.90 ft-lb/in

@Thickness 0.125 in
ASTM D256