Ovation Polymers Nemcon™ E PK DP104 Polyetheretherketone, Carbon Fiber Reinforced

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Ovation Polymers
Trade Name Nemcon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Nemcon™ E PK DP104 Polyetheretherketone, Carbon Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nemcon™ E PK DP104 is a carbon fiber reinforced polyetheretherketone, characterized by high strength, stiffness, consistent moldabiliity, and exceptional thermal resistance.All properties after 48hrs conditioning at 23°C/50% RH
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 200 MPa
29000 psi
50 mm/min; ASTM D638
Elongation at Break 2.0 %
2.0 %
50 mm/min; ASTM D638
Tensile Modulus 19.54 GPa
2834 ksi
50 mm/min; ASTM D638
Flexural Strength 320 MPa
46400 psi
1.3 mm/min; ASTM D790
Flexural Modulus 18.6 GPa
2700 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.881 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 332 °C

@Thickness 3.20 mm
630 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 1000 ohm
1000 ohm
ASTM D257