Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 1600 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 10.0 - 11.0 GPa
1450 - 1600 ksi
ASTM D790
Prodways PLASTCure Rigid 10 500 3D Printing Polymer
Superior thermo-mechanical properties.Suitable for the manufacture of parts that require thermal stability, extreme accuracy and quick turnaround. Exceptional for parts that are designed for wind tu..
Flexural Modulus 8.00 - 11.0 GPa
1160 - 1600 ksi
Compression; ISO 178
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
Flexural Modulus 9.00 - 11.0 GPa
1310 - 1600 ksi
Injection; ISO 178
Raschig Group AMPLA® 2000 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve..
Flexural Modulus 9.00 - 11.0 GPa
1310 - 1600 ksi
Compression; ISO 178
Raschig Group MELOPAS® 156 MF Melamine
Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200..
Flexural Modulus 1.57 - 11.0 GPa
228 - 1600 ksi
Average value: 5.37 GPa Grade Count:127
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Flexural Modulus 0.00800 - 11.0 GPa
1.16 - 1600 ksi
Average value: 8.29 GPa Grade Count:234
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Flexural Modulus 4.80 - 11.0 GPa
696 - 1600 ksi
Average value: 8.55 GPa Grade Count:5
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i..
Flexural Modulus 2.07 - 11.0 GPa
300 - 1600 ksi
Average value: 3.68 GPa Grade Count:7
Overview of materials for Polyphenylene Ether, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values ..
Flexural Modulus 4.80 - 11.0 GPa
696 - 1600 ksi
Average value: 7.41 GPa Grade Count:17
Overview of materials for Phenolic, Novolac, Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu..
Flexural Modulus 7.00 - 11.0 GPa
1020 - 1600 ksi
Average value: 9.38 GPa Grade Count:8
Overview of materials for Phenolic, Novolac, Fabric Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values ..
Flexural Modulus 8.96 - 11.0 GPa
1300 - 1600 ksi
ASTM D790
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Flexural Modulus 8.96 - 11.0 GPa
1300 - 1600 ksi
ASTM D790
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Flexural Modulus 8.96 - 11.0 GPa
1300 - 1600 ksi
ASTM D790
Mar-Bal MB2000-5 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Flexural Modulus 9.65 - 11.0 GPa
1400 - 1600 ksi
ASTM D790
Mar-Bal MB3000-15 Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Flexural Modulus 9.00 - 11.0 GPa
1310 - 1600 ksi
ISO 178
Vyncolit X681 Novolac Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica..
Flexural Modulus 9.65 - 11.0 GPa
1400 - 1600 ksi
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers
BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit..
Flexural Modulus 9.65 - 11.0 GPa
1400 - 1600 ksi
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound
BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o..
Flexural Modulus 1.38 - 11.0 GPa
200 - 1600 ksi
Average value: 3.70 GPa Grade Count:107
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Flexural Modulus 2.34 - 11.0 GPa
340 - 1600 ksi
Average value: 5.09 GPa Grade Count:11
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and ..
Flexural Modulus 1.72 - 11.0 GPa
250 - 1600 ksi
Average value: 4.23 GPa Grade Count:28
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max..
Flexural Modulus 9.50 - 11.0 GPa

@Temperature 80.0 - 80.0 °C
1380 - 1600 ksi

@Temperature 176 - 176 °F
Average value: 10.2 GPa Grade Count:4
Overview of materials for Polypropylene with 60% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i..
Flexural Modulus 0.134 - 11.0 GPa
19.4 - 1600 ksi
Average value: 1.39 GPa Grade Count:816
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..
Flexural Modulus 9.65 - 11.0 GPa
1400 - 1600 ksi
Bulk Molding Compounds BMC T40(20) Die Casting Replacement Grade Molding Compound
BMC T40(20) was formulated as a direct replacement for aluminum die casting applications. T40(20) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma..
Flexural Modulus 9.00 - 11.0 GPa
1310 - 1600 ksi
ISO 178
Bulk Molding Compounds tetra-DUR F 4306 Bulk Molding Compound
Mechanical high grade standard productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion pr..
Copyright © lookpolymers.com All Rights Reserved