Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.50 - 7.58 GPa | 218 - 1100 ksi | Average value: 2.31 GPa Grade Count:37 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Flexural Modulus | 3.17 - 7.58 GPa | 460 - 1100 ksi | Average value: 4.24 GPa Grade Count:14 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Flexural Modulus | 2.41 - 7.58 GPa | 350 - 1100 ksi | Average value: 5.37 GPa Grade Count:7 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Modulus | 1.72 - 7.58 GPa | 250 - 1100 ksi | Average value: 2.46 GPa Grade Count:14 |
Overview of materials for Nylon 612 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app.. |
|||
Flexural Modulus | 6.21 - 7.58 GPa | 900 - 1100 ksi | |
Bulk Molding Compounds BMC HT12-1024 Automotive Grade Molding compound BMC HT12-1024 is a high temp wear resistant molding compound designed for automotive brush holders. It is listed under Ford WS-MSD-A. It can be injection or transfer molded.Information provided by.. |
|||
Flexural Modulus | 1.90 - 7.58 GPa | 276 - 1100 ksi | Average value: 3.56 GPa Grade Count:33 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |