Material Notes:
Description: Nylene® CX 3451 is a translucent specialty nylon. CX3451 is FDA/NSF approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 1.72 GPa
250 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 195 °C
383 °F
ASTM D3418