Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87160 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES LNP COLORCOMP* JX91550 is an unfilled Polyethersulfone. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES (Asia Pacific) LNP COLORCOMP* JX91550 is a compound based on Polyethersulfone resin containing Unfilled Custom Color. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP FARADEX DX11003 PC (Europe-Africa-Middle East) LNP FARADEX DX11003 is a compound based on Polycarbonate resin potentially suitable to meet high frequency electromagnetic absorption requirments. The compound is also an excellent candidate for man.. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ISO 178 |
FKuR Kunststoff Bio-Flex® S 6540 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ISO 178 |
FKuR Kunststoff Biograde® C 6509 CL Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Flexural Modulus | 2.89 GPa | 420 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN333MS Low Friction Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Asia Pacific) LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Europe-Africa-Middle East) LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP LX00430 PEEK LNP* LUBRICOMP* LX00430 is a compound based on Pelyetheretherketone containing Proprietary Fillers. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Asia Pacific) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Europe-Africa-Middle East) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DD0009E PC LNP* STAT-KON* DD0009E is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant, Easy Molding. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX96717C PC LNP STAT-KON* DX96717C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX98477 PC LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp KB005 Acetal Copolymer LNP THERMOCOMP* KB005 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl HS1000X PPE+PS PPE+PS blend. 13% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL 746C f1. Radiant Panel listing. Dielectric strength. Dimensional stability. Suitable for .. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC (Asia Pacific) LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East) A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.89 GPa | 419 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.89 GPa @Thickness 3.20 mm |
420 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical |