Material Notes:
Features: Antistatic, Medium Clarity, Good FlowUses: Household Goods, KitchenwareApprovals: FDA 21 CFR 176.170(c), Table 2, Cond. B, C, D, E, F, G and HProcessing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 92
92
ASTM D785
Tensile Strength, Yield 29.6 MPa
4300 psi
Type I, 2 in/min; ASTM D638
Elongation at Break 12 %
12 %
Type I, 2 in/min; ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256