Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Paxon™ BA50-120 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Exxon Chemical
Trade Name Paxon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Paxon™ BA50-120 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: BA50-120 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesAntistatic: NoApplications: Agriculture ProductsAutomotive FittingsAutomotive Fuel Tanks DrumsFood packagingHeavy Gauge Sheet Large Part Blow MoldingPalletsPortable Fuel TanksSmall Engine Fuel Tanks Thermoformed PartsInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM D4883
ESCR 100% Igepal® >= 800 hour
>= 800 hour
ASTM D1693 Condition B
Melt Flow 11 g/10 min
11 g/10 min
190 / 21.6 (HLMI); ASTM D1238
<= 0.10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
<= 0.10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Break 1100 %
1100 %
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
Tensile Impact Strength 210 kJ/m²
100 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 204 °C
400 °F
Descriptive Properties Value Comments
Features Thermal Stabilizer
Copyright © lookpolymers.com All Rights Reserved