Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M. Holland Company PP100 Polypropylene Homopolymer, General Purpose

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer M. Holland Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company PP100 Polypropylene Homopolymer, General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High clarityHomopolymerGood melt strengthHigh tensile strengthApplications: Thin-walled partsSheetStrapping
Physical Properties Metric English Comments
Melt Flow 1.6 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.6 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Forms Pellets
Processing Methods Blow molding, extrusion, sheet extrusion, thermoforming
Copyright © lookpolymers.com All Rights Reserved