Features:medium flowcontains clarifying agentexcellent clarityApplications:storage boxesvialscontainersFormer A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Melt Index of Compound 12 g/10 min

@Temperature 230 °C
12 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 32.69 MPa
4742 psi
50 mm/min; ASTM D638
Elongation at Yield 12 %
12 %
50 mm/min; ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
1.3 mm/min, 1% Secant; ASTM D790
Izod Impact, Notched 0.587 J/cm

@Temperature 22.8 °C
1.10 ft-lb/in

@Temperature 73.0 °F
ASTM D256