Material Notes:
Homopolymer, FDA compliant.Features: Low water carryover.Applications: Extrusion: slit film and oriented fibers.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 3.5 g/10 min
3.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 39.0 MPa
5660 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.59 GPa
231 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
23° C; ASTM D256
Gardner Impact 17.0 J
12.5 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648