Extrusion Grade Pellets. GMP # 002. Property values below represent typical values. Information provided by Engineered Plastics Corporation.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Melt Flow 1.0 g/10 min
1.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.7 MPa
4600 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Modulus 1.59 GPa
231 ksi
ASTM D790
Izod Impact, Notched 4.30 J/cm
8.06 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
Annealed; ASTM Data
103 °C
217 °F
Unannealed; ASTM Data
Vicat Softening Point 103 °C
217 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in