Material Notes:
H03W-01 (formerly Fortilene® HG3253) belongs to the new generation of polypropylenes produced by gas phase polymerization. This nominal 4 melt flow index product is specifically designed for fiber applications which require low water carryover characteristics coupled with good melt and thermal stability in the finished product. Specific applications for HG3253 include cordage, carpet backing, industrial fabrics and geotextiles. This material meets the FDA requirements of 21CFR 177.1520. Data provided by the manufacturer, Solvay Polymers, Inc.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D4883
Melt Flow 4.0 g/10 min
4.0 g/10 min
Condition not specified. ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
ASTM D2240
Tensile Strength, Yield 33.8 MPa
4900 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.59 GPa
231 ksi
1% Secant at 0.05 in/min; ASTM D790
Izod Impact, Notched 0.220 J/cm
0.412 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ASTM D3418
Crystallization Temperature 110 °C
230 °F
ASTM D3418