Material Notes:
Description: Multi Purpose, Good Color and Process StabilityApplications: Suggested Uses Include Housewares, Patio Furniture, ClosuresThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength 35.9 MPa
5200 psi
2 in/min; ASTM D638
Flexural Modulus 1.59 GPa
230 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256A
Users viewing this material also viewed the following: