Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 0.193 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.193 GPa
28.0 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 9502 BLK , 7% Filler Content
The moisture content is 0.02%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.193 GPa
28.0 ksi
3 pt. secant; ASTM D790
Chevron Phillips KN 230 LDPE Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ESCRApplications:Houseware..
Flexural Modulus 0.193 GPa
28.0 ksi
3 pt. secant; ASTM D790
Chevron Phillips KN 230B LDPE Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ..
Flexural Modulus 0.193 GPa
28.0 ksi
3 pt. secant; ASTM D790
Chevron Phillips Marlex® 1409 Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications..
Flexural Modulus 0.193 GPa
28.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 1390P Polyethylene  (discontinued **)
Low-density polyethylene 1390P is used primarily in extrusion-coating applications that require fast line speeds and relatively low coating weights. When compared with other low-density polyethylen..
Flexural Modulus 0.193 GPa
28.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 808E Polyethylene  (discontinued **)
Low density polyethylene 808E is a general-purpose formulation used general-purpose extrusion. Under regulations administered by the US FDA, 808E may lawfully be used as articles or components of a..
Flexural Modulus 0.193 GPa
28.0 ksi
ASTM D790
Multibase Multi-Flex® A 8620 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Thermal Stability, GoodOzone Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automotive Interior PartsCoverings, ProtectiveInformation provide..
Flexural Modulus 0.193 GPa
28.0 ksi
ASTM D790
Multibase Multi-Flex® D 3104 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI..
Flexural Modulus 0.193 GPa
28.0 ksi
3 pt. secant; ASTM D790
Chevron Phillips Marlex® 1412 Injection Molding Resin
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications..
Flexural Modulus 0.193 - 0.248 GPa
28.0 - 36.0 ksi
ASTM D790
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Copyright © lookpolymers.com All Rights Reserved