Mechanical Properties Metric English Comments
Flexural Modulus 0.193 - 0.248 GPa
28.0 - 36.0 ksi
ASTM D790
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..