Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® A 8620 TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 8620 TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Chemical Resistance, Good Thermal Stability, GoodOzone Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automotive Interior PartsCoverings, ProtectiveInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM 792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
10 seconds; ASTM D2240
Tensile Strength, Yield 12.4 MPa
1800 psi
Elastic; ASTM D638
Elongation at Break 650 %
650 %
ASTM D638
Flexural Modulus 0.193 GPa
28.0 ksi
ASTM D790
Tear Strength 50.8 kN/m
290 pli
ASTM D624
Users viewing this material also viewed the following: