Multibase Multi-Flex® TPE A 9502 BLK , 7% Filler Content

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 9502 BLK , 7% Filler Content.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The moisture content is 0.02%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Melt Flow 15.51 g/10 min
15.51 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 91.4
91.4
10 sec; ASTM D-2240
Tensile Strength, Ultimate 14.5 MPa
2100 psi
ASTM D412
Elongation at Break 675 %
675 %
ASTM D412
Flexural Strength 6.30 MPa
914 psi
Flexural Modulus 0.193 GPa
28.0 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 71.5 kN/m
408 pli
ASTM D624
Users viewing this material also viewed the following: