Chevron Phillips 4522 LDPE Shrink and Heavy Duty Packaging Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips 4522 LDPE Shrink and Heavy Duty Packaging Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: HomopolymerCharacteristics: Excellent Tensile Strength, Excellent Impact Strength, Very Good Tear Resistance, Very Good Abrasion Resistance, No Slip, No AntiblockApplications:Pallet Shrink Wrap, Heavy Duty PackagingProcessing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 3:1.Film properties below based on film thickness of 76 µm.Data provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 0.50 g/10 min
0.50 g/10 min
Condition E; ASTM D 1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.170 GPa
24.7 ksi
ASTM D882
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Coefficient of Friction >= 1.0
>= 1.0
ASTM D1894
Dart Drop 2.80 g/micron
71.1 g/mil
F<sub>50</sub>; 2 in. dart/60 in. drop height; ASTM D 1709
Optical Properties Metric English Comments
Haze 9.5 %
9.5 %
ASTM D2457
Gloss 59 %
59 %
at 45°. ASTM D 2457
95 %
95 %
at 60°. ASTM D 2457
Processing Properties Metric English Comments
Melt Temperature 210 °C
410 °F