Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® LD-314 EVA Packaging Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD-314 EVA Packaging Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low temperature properties versus homopolymer clarity film resins.Applications: Frozen food packaging; Freezer bags; Other food packaging including light duty produce bags, etc.; Laminating films; Packaging applications where good toughness, heat sealability and high clarity are required. Data for film properties below based on 1.25 mil film.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
Exxon Method
Thickness 31.8 microns
1.25 mil
Melt Flow 2.2 g/10 min
2.2 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 8.30 MPa
1200 psi
ASTM D882
Film Tensile Strength at Yield, TD 8.30 MPa
1200 psi
ASTM D882
Film Elongation at Break, MD 200 %
200 %
ASTM D882
Film Elongation at Break, TD 600 %
600 %
ASTM D882
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Elmendorf Tear Strength MD 375 g
375 g
ASTM D1922
Elmendorf Tear Strength TD 100 g
100 g
ASTM D1922
Elmendorf Tear Strength, MD 11.8 g/micron
300 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 3.15 g/micron
80.0 g/mil
ASTM D1922
Dart Drop 3.15 g/micron
80.0 g/mil
F50; ASTM D1709
Dart Drop Test 100 g
0.221 lb
F50; ASTM D-1709
Film Tensile Strength at Break, MD 24.0 MPa
3480 psi
ASTM D882
Film Tensile Strength at Break, TD 19.0 MPa
2760 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 106 °C
223 °F
Exxon Method
Optical Properties Metric English Comments
Haze 5.0 %
5.0 %
ASTM D1003
Gloss 75 %
75 %
45°, ASTM D-2457
Copyright © lookpolymers.com All Rights Reserved