Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips MarFlex® 1122 Clarity, Liner Grade Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Liner Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name MarFlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips MarFlex® 1122 Clarity, Liner Grade Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: HomopolymerCharacteristics: Good Impact, No slip, No antiblock, Good processability, Good sealabilityApplications:Liners, Trash bagsProcessing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 2:1.Film properties below based on film thickness of 31.8 µm.Data provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
Condition E; ASTM D 1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Coefficient of Friction >= 1.0
>= 1.0
ASTM D1894
Dart Drop 2.80 g/micron
71.1 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Optical Properties Metric English Comments
Haze 8.0 %
8.0 %
ASTM D2457
Gloss 50 %
50 %
at 45°. ASTM D 2457
80 %
80 %
at 60°. ASTM D 2457
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 193 °C
379 °F