Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 89.6 MPa | 13000 psi | ASTM D732 |
Quadrant EPP Duratron® PI D7015G PI Bearing Grade Polyimide (ASTM Product Data Sheet) |
|||
Shear Strength | 89.6 MPa | 13000 psi | Notched Compression In-plane, Dry, RT; ASTM D3846-02 |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin 4581 Astroquartz III Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |
|||
Shear Strength | 89.6 MPa | 13000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Shear Strength | 89.6 MPa @Thickness 3.17 mm |
13000 psi @Thickness 0.125 in |
|
Industrial Laminates/Norplex MC223 Cotton Fabric Description: Grade MC223 is a medium weave cotton phenolic composite that is specifically formulated to meet MIL-P-18324.Typical applications include pintle and stave-type bearings for rudder shafts.. |
|||
Shear Strength | 89.6 MPa @Thickness 15.7 mm |
13000 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP315 Cotton Fabric Description: Canvas phenolic laminate with graphite added as a solid lubricant. This material has improved wear properties under certain conditions. Material is conductive to electricity and should .. |
|||
Shear Strength | 89.6 MPa @Thickness 15.7 mm |
13000 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP319 Cotton Fabric Base Laminate Description: Bleached canvas combined with phenolic resin and graphite lubricant. Better moisture resistance and machining characteristics than NP315. |
|||
Shear Strength | 89.6 MPa @Thickness 15.7 mm |
13000 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP329 Cotton Fabric Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, .. |
|||
Shear Strength | 89.6 MPa @Thickness 15.7 mm |
13000 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP639 Paper Base Laminate Description: Economical paper reinforced laminate developed with capacity to withstand temperatures to 150° C without blistering. High compressive strength and low moisture absorption.Thickness T.. |
|||
Shear Strength | 89.6 MPa | 13000 psi | Axial; ASTM D732 |
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Shear Strength | 89.6 MPa @Thickness 3.17 mm |
13000 psi @Thickness 0.125 in |
|
Industrial Laminates/Norplex MC330 Cotton Fabric Description: Grade MC330 is a cotton cloth/phenolic resin composite which is specially processed to be used in cryogenic applications. Such applications include spacers for installation of liquid ox.. |
|||
Shear Strength | 89.6 MPa @Thickness 15.7 mm |
13000 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP310U Cotton Fabric Description: Utility grade canvas phenolic with properties similar to NP310E.Not certifiable to NEMA due to low crosswise flexural strength. Previously designated NP310C.Thickness Tested: 0.062", 0... |
|||
Shear Strength | 89.6 MPa | 13000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Shear Strength | 89.6 MPa | 13000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Shear Strength | 89.6 MPa | 13000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Shear Strength | 89.6 MPa | 13000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Shear Strength | 89.6 MPa | 13000 psi | Compression interlaminar; RT |
Hexcel® HexPly® F155 Epoxy Resin, T2C145 Carbon Tape Hexcel designation: TXX145-12"-F155; Various fibersInformation provided by HexCel |
|||
Shear Strength | 89.6 MPa | 13000 psi | Ultimate |
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Shear Strength | 89.6 MPa | 13000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
Shear Strength | 89.6 MPa | 13000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
Shear Strength | 89.6 MPa | 13000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |