Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® F155 Epoxy Resin, T2C145 Carbon Tape

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F155 Epoxy Resin, T2C145 Carbon Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexcel designation: TXX145-12"-F155; Various fibersInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.62 MPa

@Temperature 24.0 °C
670 psi

@Temperature 75.2 °F
Flatwise TS
1710 MPa

@Temperature 71.0 °C
248000 psi

@Temperature 160 °F
1834 MPa

@Temperature 24.0 °C
266000 psi

@Temperature 75.2 °F
Tensile Modulus 119 GPa

@Temperature 71.0 °C
17300 ksi

@Temperature 160 °F
126.2 GPa

@Temperature 24.0 °C
18300 ksi

@Temperature 75.2 °F
Compressive Yield Strength 1172 MPa

@Temperature 71.0 °C
170000 psi

@Temperature 160 °F
1331 MPa

@Temperature 24.0 °C
193000 psi

@Temperature 75.2 °F
Compressive Modulus 117 GPa

@Temperature 71.0 °C
17000 ksi

@Temperature 160 °F
Shear Strength 89.6 MPa
13000 psi
Compression interlaminar; RT
71.7 MPa

@Temperature 71.0 °C
10400 psi

@Temperature 160 °F
Compression interlaminar
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.014
Laminate
Dry Resin Content (%) 38-40
Prepreg
Fiber Volume (%) 57
Laminate
Flow (%) 4-16