Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Industrial Laminates/Norplex MC330 Cotton Fabric

Category Polymer , Thermoset , Phenolic
Manufacturer Industrial Laminates/Norplex
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industrial Laminates/Norplex MC330 Cotton Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Grade MC330 is a cotton cloth/phenolic resin composite which is specially processed to be used in cryogenic applications. Such applications include spacers for installation of liquid oxygen apparatus where temperatures are as low as minus 320°F.Grade MC330 complies with MIL-I-24768/16.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0530 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90 - 110

@Thickness 3.17 mm
90 - 110

@Thickness 0.125 in
Tensile Strength, Yield 89.6 MPa

@Thickness 3.17 mm
13000 psi

@Thickness 0.125 in
LW
Flexural Strength 276 MPa

@Thickness 3.17 mm
40000 psi

@Thickness 0.125 in
LW
Compressive Strength 145 MPa

@Thickness 3.17 mm
21000 psi

@Thickness 0.125 in
Flatwise
Shear Strength 89.6 MPa

@Thickness 3.17 mm
13000 psi

@Thickness 0.125 in
Izod Impact, Unnotched 0.998 J/cm

@Thickness 3.17 mm
1.87 ft-lb/in

@Thickness 0.125 in
LW, E-48/50
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved