Industrial Laminates/Norplex NP315 Cotton Fabric

Category Polymer , Thermoset , Phenolic
Manufacturer Industrial Laminates/Norplex
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industrial Laminates/Norplex NP315 Cotton Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Canvas phenolic laminate with graphite added as a solid lubricant. This material has improved wear properties under certain conditions. Material is conductive to electricity and should no be used where this is detrimental to the application.Thickness Tested: 0.062", 0.125", and 0.500"
Physical Properties Metric English Comments
Specific Gravity 1.35 - 1.45 g/cc

@Thickness 1.57 mm
1.35 - 1.45 g/cc

@Thickness 0.0620 in
ASTM D792
Moisture Absorption at Equilibrium 2.2 %

@Thickness 1.57 mm
2.2 %

@Thickness 0.0620 in
ASTM D229
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80 - 100

@Thickness 1.57 mm
80 - 100

@Thickness 0.0620 in
ASTM D785
Tensile Strength, Yield 48.3 MPa

@Thickness 1.57 mm
7000 psi

@Thickness 0.0620 in
CW; ASTM D638
68.9 MPa

@Thickness 1.57 mm
10000 psi

@Thickness 0.0620 in
LW; ASTM D638
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
CW; ASTM D229
8.27 GPa

@Thickness 1.57 mm
1200 ksi

@Thickness 0.0620 in
LW; ASTM D229
Flexural Strength 103 MPa

@Thickness 1.57 mm
15000 psi

@Thickness 0.0620 in
CW; ASTM D790
131 MPa

@Thickness 1.57 mm
19000 psi

@Thickness 0.0620 in
LW; ASTM D790
Compressive Strength 262 MPa

@Thickness 12.7 mm
38000 psi

@Thickness 0.500 in
ASTM D695
Shear Strength 89.6 MPa

@Thickness 15.7 mm
13000 psi

@Thickness 0.620 in
ASTM D732
Izod Impact, Unnotched 0.747 J/cm

@Thickness 12.7 mm
1.40 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
0.908 J/cm

@Thickness 12.7 mm
1.70 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
10.0 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 24.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
13.3 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Maximum Service Temperature, Air 145 °C
293 °F
Flammability, UL94 HB

@Thickness 1.57 mm
HB

@Thickness 0.0620 in
Descriptive Properties Value Comments
Bond Strength 1800 lb
0.5", ASTM D229
Color Natural, Black