Type P-VSB-32 (Union Carbide) Carbon Fiber

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Type P-VSB-32 (Union Carbide) Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pitch fibers are prepared by heating aromatic compounds above 350°C. A dehydrogenation condensation reaction occurs to form planar aromatic molecules which aggregate into a liquid crystalline phase (a mesophase). Once the mesophase content has reached about 40%, a phase inversion occurs and this anisotropic material becomes the continuous phase.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2000 MPa
290000 psi
Fiber only. Composites containing this fiber may have tensile strength of 1000 MPa.
Modulus of Elasticity 220 GPa
31900 ksi
or 350 GPa for fiber
Shear Strength 31.0 MPa
4500 psi
Interlaminar shear.