Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Resin Density
2.10 g/cc
0.0759 lb/in³
Fibre Density
Mechanical Properties Metric English Comments
Tensile Strength, Yield 400 MPa
58000 psi
90º, RT, Dry; EN2561
320 MPa

@Temperature 130 °C
46400 psi

@Temperature 266 °F
90º, Wet; EN2561
370 MPa

@Temperature 23.0 °C
53700 psi

@Temperature 73.4 °F
90º, Wet; EN2561
Tensile Modulus 38.0 GPa
5510 ksi
90º, RT, Dry; EN2561
37.0 GPa

@Temperature 23.0 °C
5370 ksi

@Temperature 73.4 °F
90º, Wet; EN2561
37.0 GPa

@Temperature 130 °C
5370 ksi

@Temperature 266 °F
90º, Wet; EN2561
Compressive Yield Strength 650 MPa
94300 psi
90º, RT, Dry; EN2850 Type B
390 MPa

@Temperature 130 °C
56600 psi

@Temperature 266 °F
90º, Wet; EN2850 Type B
590 MPa

@Temperature 23.0 °C
85600 psi

@Temperature 73.4 °F
90º, Wet; EN2850 Type B
Compressive Modulus 37.0 GPa
5370 ksi
90º, RT, Dry; EN2850 Type B
36.0 GPa

@Temperature 130 °C
5220 ksi

@Temperature 266 °F
90º, Wet; EN2850 Type B
38.0 GPa

@Temperature 23.0 °C
5510 ksi

@Temperature 73.4 °F
90º, Wet; EN2850 Type B
Shear Modulus 3.50 GPa
508 ksi
In-Plane, RT, Dry; EN6031
2.40 GPa

@Temperature 130 °C
348 ksi

@Temperature 266 °F
In-Plane, Wet; EN6031
Shear Strength 68.0 MPa
9860 psi
90º, ILSS Short Beam, RT, Dry; EN2563
79.0 MPa
11500 psi
In-Plane, RT, Dry; EN6031
31.0 MPa

@Temperature 150 °C
4500 psi

@Temperature 302 °F
90º, ILSS Short Beam, Wet; EN2563
34.0 MPa

@Temperature 130 °C
4930 psi

@Temperature 266 °F
90º, ILSS Short Beam, Wet; EN2563
48.0 MPa

@Temperature 130 °C
6960 psi

@Temperature 266 °F
In-Plane, Wet; EN6031
54.0 MPa

@Temperature 100 °C
7830 psi

@Temperature 212 °F
In-Plane, Wet; EN6031
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 - 130 °C
248 - 266 °F
Epoxy Matrix Limit
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.021
Fiber Volume (%) 42