Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 75.8 - 105 MPa | 11000 - 15300 psi | Average value: 92.4 MPa Grade Count:7 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |