Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Water Absorption 0.30 %
0.30 %
IMMERSION, 24 HRS.; ASTM D570 2
Water Absorption at Saturation 7.0 %
7.0 %
ASTM D570 2
Mechanical Properties Metric English Comments
Tensile Strength 89.6 MPa
13000 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Tensile Modulus 3.62 GPa
525 ksi
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 3.24 GPa
470 ksi
ASTM D790
Compressive Strength 93.1 MPa

@Strain 10.0 %,
Temperature 22.8 °C
13500 psi

@Strain 10.0 %,
Temperature 73.0 °F
ASTM D695
Compressive Modulus 3.59 GPa
520 ksi
ASTM D695
Shear Strength 75.8 MPa
11000 psi
ASTM D732
Thermal Properties Metric English Comments
Thermal Conductivity 0.245 W/m-K
1.70 BTU-in/hr-ft²-°F
ASTM E1530-11
Melting Point 260 °C
500 °F
1.0e+6 Hz; ASTM D3418
Electrical Properties Metric English Comments
Dielectric Constant 3.6
3.6
ASTM D150
Dissipation Factor 0.030
0.030
1.0e+6 Hz; ASTM D150