Polymer Property : Elmendorf Tear Strength TD = 140 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 140 g
140 g
Eastman E6838-795F Polyethylene  (discontinued **)
E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag..
Elmendorf Tear Strength TD 140 g
140 g
Eastman E6838-796F Polyethylene  (discontinued **)
E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen..
Elmendorf Tear Strength TD 140 g
140 g
Eastman E6838-964F Polyethylene  (discontinued **)
E6838-964F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati..
Elmendorf Tear Strength TD 140 g
140 g
ASTM D1922
ExxonMobil LD 146.NH Cast Film Resin  (discontinued **)
LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength TD 140 g
140 g
ASTM D1922
ExxonMobil LD 146.NH Packaging Film Resin  (discontinued **)
LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength TD 140 g
140 g
ASTM D 1922
Total Finathene® 1288 HDPE film  (discontinued **)
Applications: Flat bottom bags, draw strings, coextruded merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plasti..
Elmendorf Tear Strength TD 140 g
140 g
ASTM D1922
NOVA Chemicals Sclair® 94E Butene LMDPE Film and Extrusion Resin
Features: Excellent processabilityGood stiffness and strengthHigh stretchability Applications: Overwrap filmNettingBlend resinInformation provided by Nova Chemicals
Elmendorf Tear Strength TD 140 g
140 g
ISO 6383-2
Inno-Comp INNOPOL® CS 5-8250 W 50% Chalk-Filled High Density Polyethylene
INNOPOL® CS 5-8250 W is a 50% chalk-filled compound based on high density polyethylene.INNOPOL® CS 5-8250 W is developed for packaging film production.All information provided by INNO-COMP.
Elmendorf Tear Strength TD 140 g
140 g
ASTM D1922
ExxonMobil LD 071.LQ Blown Film Resin
L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou..
Elmendorf Tear Strength TD 140 g
140 g
ASTM D1922
ExxonMobil LD 071.LR Blown Film Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
Elmendorf Tear Strength TD 140 g
140 g
ASTM D1922
ExxonMobil LD 313.NF Blown Film Resin
LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr..
Elmendorf Tear Strength TD 140 g
140 g
ASTM D1922
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
Elmendorf Tear Strength TD 140 g
140 g
ASTM D1922
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
Elmendorf Tear Strength TD 140 g
140 g
ASTM-D1922
Braskem F0421 D LDPE Blown Film Extrusion Polyethylene
LDPE F0421 D is a low-density polyethylene resin. It has high mechanical and impact strength and good processability, sealability, and shrinkage. It contains antioxidant and slip additives. Its appl..
Elmendorf Tear Strength TD 140 g
140 g
gF; ASTM D1922
Braskem F0421D Blown Film Extrusion Low Density Polyethylene
Shrink films; Automatic packaging of liquid products (FFS).Additives: Antiblock, DInformation provided by Braskem.
Elmendorf Tear Strength TD 140 g
140 g
Eastman D4036-F Polyethylene  (discontinued **)
D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener..
Elmendorf Tear Strength TD 140 g
140 g
Eastman E6838-963F Polyethylene  (discontinued **)
E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati..