Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 140 g | 140 g | |
Eastman E6838-795F Polyethylene
(discontinued **) E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag.. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | |
Eastman E6838-796F Polyethylene
(discontinued **) E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen.. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | |
Eastman E6838-964F Polyethylene
(discontinued **) E6838-964F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | ASTM D1922 |
ExxonMobil LD 146.NH Cast Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | ASTM D1922 |
ExxonMobil LD 146.NH Packaging Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | ASTM D 1922 |
Total Finathene® 1288 HDPE film
(discontinued **) Applications: Flat bottom bags, draw strings, coextruded merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plasti.. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | ASTM D1922 |
NOVA Chemicals Sclair® 94E Butene LMDPE Film and Extrusion Resin Features: Excellent processabilityGood stiffness and strengthHigh stretchability Applications: Overwrap filmNettingBlend resinInformation provided by Nova Chemicals |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | ISO 6383-2 |
Inno-Comp INNOPOL® CS 5-8250 W 50% Chalk-Filled High Density Polyethylene INNOPOL® CS 5-8250 W is a 50% chalk-filled compound based on high density polyethylene.INNOPOL® CS 5-8250 W is developed for packaging film production.All information provided by INNO-COMP. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | ASTM D1922 |
ExxonMobil LD 071.LQ Blown Film Resin L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou.. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | ASTM D1922 |
ExxonMobil LD 071.LR Blown Film Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | ASTM D1922 |
ExxonMobil LD 313.NF Blown Film Resin LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr.. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | ASTM D1922 |
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | ASTM D1922 |
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | ASTM-D1922 |
Braskem F0421 D LDPE Blown Film Extrusion Polyethylene LDPE F0421 D is a low-density polyethylene resin. It has high mechanical and impact strength and good processability, sealability, and shrinkage. It contains antioxidant and slip additives. Its appl.. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | gF; ASTM D1922 |
Braskem F0421D Blown Film Extrusion Low Density Polyethylene Shrink films; Automatic packaging of liquid products (FFS).Additives: Antiblock, DInformation provided by Braskem. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | |
Eastman D4036-F Polyethylene
(discontinued **) D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener.. |
|||
Elmendorf Tear Strength TD | 140 g | 140 g | |
Eastman E6838-963F Polyethylene
(discontinued **) E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |