Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 680 - 900 MPa | 98600 - 131000 psi | |
Materion Beryllium Copper Alloy 10 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17500) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Ultimate | 680 - 900 MPa | 98600 - 131000 psi | |
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17500) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Ultimate | 680 - 900 MPa | 98600 - 131000 psi | |
Materion Beryllium Copper Alloy 10 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17500) Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Ultimate | 620 - 900 MPa | 89900 - 131000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; up to 9.5 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 620 - 900 MPa | 89900 - 131000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 750 - 900 MPa | 109000 - 131000 psi | |
Materion Beryllium Copper Alloy 174 Strip; HT (TH04) Temper (UNS C17410) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Ultimate | 620 - 900 MPa | 89900 - 131000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; up to 9.5 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 620 - 900 MPa | 89900 - 131000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 620 - 900 MPa | 89900 - 131000 psi | |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 680 - 900 MPa | 98600 - 131000 psi | |
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Ultimate | 680 - 900 MPa | 98600 - 131000 psi | |
Materion Beryllium Copper Alloy 3 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Ultimate | 620 - 900 MPa | 89900 - 131000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 800 - 900 MPa | 116000 - 131000 psi | |
SSAB Tunnplat Docol® 800 DP High-strength Steel Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Ultimate | 780 - 900 MPa | 113000 - 131000 psi | |
ArcelorMittal Complex Phase Steel 800 Y500 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT780C) and electrogalvanized (HCT780C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r.. |
|||
Tensile Strength, Ultimate | 780 - 900 MPa | 113000 - 131000 psi | |
ArcelorMittal Complex Phase Steel 800 Y600 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT780C), electrogalvanized (HCT780C+ZE) and Extragal®/Galvannealed (HCT780+Z)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS .. |
|||
Tensile Strength, Ultimate | 780 - 900 MPa | 113000 - 131000 psi | |
ArcelorMittal Dual Phase 780 LCE Y450 Very high strength steel, Cold Rolled Steel Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft .. |
|||
Tensile Strength, Ultimate | 780 - 900 MPa | 113000 - 131000 psi | |
ArcelorMittal Dual Phase 780 LCE Y500 Very high strength steel, Cold Rolled Steel Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft .. |
|||
Tensile Strength, Ultimate | 780 - 900 MPa | 113000 - 131000 psi | |
ArcelorMittal TRIP 780 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT780T), electrogalvanized (HCT780T+ZE) and Extragal®/Galvannealed (HCT780T+Z/+ZZF)Description: TRIP steels offer an outstanding combination of strength and d.. |
|||
Tensile Strength, Ultimate | 780 - 900 MPa | 113000 - 131000 psi | |
ArcelorMittal Dual Phase 780 Y450 Very high strength steel, Cold Rolled Steel Available in the following: HCT780X (uncoated), HCT780X+ZE (electrogalvanized) and HCT780X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a.. |
|||
Tensile Strength, Ultimate | 780 - 900 MPa | 113000 - 131000 psi | |
ArcelorMittal Dual Phase 780 Y500 Very high strength steel, Cold Rolled Steel Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft .. |
|||
Tensile Strength, Ultimate | 680 - 900 MPa | 98600 - 131000 psi | |
Materion Beryllium Copper Alloy 3 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17510) Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials .. |
|||
Tensile Strength, Ultimate | 680 - 900 MPa | 98600 - 131000 psi | |
Materion Beryllium Copper Alloy 3 Strip; AT (TF00) Temper (UNS C17510) Treatment required for max strength: 2-3 hrs @ 480ºC or Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 94%Stress Relaxation after 1000 hrs @ 200°C: 72%Formability Ratio.. |
|||
Tensile Strength, Ultimate | 680 - 900 MPa | 98600 - 131000 psi | |
Materion Beryllium Copper Alloy 3 Tube; AT (TF00) Temper; All Sizes (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc... |