Polymer Property : Tensile Strength, Ultimate = 131000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 10 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17500)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17500)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 10 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Tensile Strength, Ultimate 620 - 900 MPa
89900 - 131000 psi
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; up to 9.5 mm Thickness (UNS C17000)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 620 - 900 MPa
89900 - 131000 psi
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17000)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 750 - 900 MPa
109000 - 131000 psi
Materion Beryllium Copper Alloy 174 Strip; HT (TH04) Temper (UNS C17410)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R..
Tensile Strength, Ultimate 620 - 900 MPa
89900 - 131000 psi
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; up to 9.5 mm Thickness (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 620 - 900 MPa
89900 - 131000 psi
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 620 - 900 MPa
89900 - 131000 psi
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; up to 9.5 mm o.d. (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17510)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 3 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17510)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Ultimate 620 - 900 MPa
89900 - 131000 psi
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17300)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 800 - 900 MPa
116000 - 131000 psi
SSAB Tunnplat Docol® 800 DP High-strength Steel
Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm.Data provided by SSAB Tunnplat.
Tensile Strength, Ultimate 780 - 900 MPa
113000 - 131000 psi
ArcelorMittal Complex Phase Steel 800 Y500 Very high strength steel, Cold Rolled Steel
Available in the following: uncoated (HCT780C) and electrogalvanized (HCT780C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r..
Tensile Strength, Ultimate 780 - 900 MPa
113000 - 131000 psi
ArcelorMittal Complex Phase Steel 800 Y600 Very high strength steel, Cold Rolled Steel
Available in the following: uncoated (HCT780C), electrogalvanized (HCT780C+ZE) and Extragal®/Galvannealed (HCT780+Z)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS ..
Tensile Strength, Ultimate 780 - 900 MPa
113000 - 131000 psi
ArcelorMittal Dual Phase 780 LCE Y450 Very high strength steel, Cold Rolled Steel
Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft ..
Tensile Strength, Ultimate 780 - 900 MPa
113000 - 131000 psi
ArcelorMittal Dual Phase 780 LCE Y500 Very high strength steel, Cold Rolled Steel
Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft ..
Tensile Strength, Ultimate 780 - 900 MPa
113000 - 131000 psi
ArcelorMittal TRIP 780 Very high strength steel, Cold Rolled Steel
Available in the following: uncoated (HCT780T), electrogalvanized (HCT780T+ZE) and Extragal®/Galvannealed (HCT780T+Z/+ZZF)Description: TRIP steels offer an outstanding combination of strength and d..
Tensile Strength, Ultimate 780 - 900 MPa
113000 - 131000 psi
ArcelorMittal Dual Phase 780 Y450 Very high strength steel, Cold Rolled Steel
Available in the following: HCT780X (uncoated), HCT780X+ZE (electrogalvanized) and HCT780X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a..
Tensile Strength, Ultimate 780 - 900 MPa
113000 - 131000 psi
ArcelorMittal Dual Phase 780 Y500 Very high strength steel, Cold Rolled Steel
Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft ..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 3 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17510)
Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials ..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 3 Strip; AT (TF00) Temper (UNS C17510)
Treatment required for max strength: 2-3 hrs @ 480ºC or Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 94%Stress Relaxation after 1000 hrs @ 200°C: 72%Formability Ratio..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 3 Tube; AT (TF00) Temper; All Sizes (UNS C17510)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc...