Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 680 MPa
98600 psi
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
Tensile Strength, Ultimate 680 MPa

@Temperature 100 °C
98600 psi

@Temperature 212 °F
EN min.; EN 10002-5
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 10 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17500)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17500)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 10 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Tensile Strength, Ultimate 680 - 760 MPa
98600 - 110000 psi
Materion Beryllium Copper Alloy 190 Strip; AM (TM00) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Tensile Strength, Ultimate 680 - 830 MPa
98600 - 120000 psi
Materion Beryllium Copper Alloy 25 Strip; H (TD04) Temper (UNS C17200)
Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1Formability Ratio (bad Way): 2.9Superficial Hardness: 30T 79-83Tabulated properties appl..
Tensile Strength, Ultimate 680 - 830 MPa
98600 - 120000 psi
Materion Beryllium Copper Alloy 3 Forgings & Extrusions; AT (TF00) Temper (UNS C17510)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17510)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 3 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17510)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Ultimate >= 680 MPa
>= 98600 psi
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM00 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R..
Tensile Strength, Ultimate 680 MPa
98600 psi
Typical after Solution Annealing
Industeel SIRIUS S15 Rare Earth Containing Heat Resistant Steel
CLI SIRIUS S15 grade is a fully austenitic stainless steel containing 21 Cr, 1.7 Si, 0.17 N and Rare Earth elements (Cerium, Lanthanum,...etc) which make the alloy particularly well designed for hig..
Tensile Strength, Ultimate 680 MPa
98600 psi
Typical
TIMET 75A CP Titanium (ASTM Grade 4)
Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4901. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specification BS TA. 6.Features..
Tensile Strength, Ultimate 680 - 740 MPa
98600 - 107000 psi
CLAL-MSX DECLAFOR® 1015 TD4 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Tensile Strength, Ultimate 680 MPa
98600 psi
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 30% cold work (ASTM XM-8; UNS S43035)
Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi..
Tensile Strength, Ultimate >= 680 MPa
>= 98600 psi
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34
Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 3 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17510)
Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials ..
Tensile Strength, Ultimate 680 - 830 MPa
98600 - 120000 psi
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; AT (TF00) Temper (UNS C17500)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc...
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 3 Strip; AT (TF00) Temper (UNS C17510)
Treatment required for max strength: 2-3 hrs @ 480ºC or Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 94%Stress Relaxation after 1000 hrs @ 200°C: 72%Formability Ratio..
Tensile Strength, Ultimate 680 - 900 MPa
98600 - 131000 psi
Materion Beryllium Copper Alloy 3 Tube; AT (TF00) Temper; All Sizes (UNS C17510)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc...