Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 620 - 870 MPa | 89900 - 126000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 9.5 to 25 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 620 - 870 MPa | 89900 - 126000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 620 - 900 MPa | 89900 - 131000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 620 - 870 MPa | 89900 - 126000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 620 - 900 MPa | 89900 - 131000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; up to 9.5 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | >= 620 MPa | >= 89900 psi | |
Kobe Steel KS3-2.5 Alpha-Beta Titanium Alloy, ASTM Gr. 9, Annealed Nominal Composition: Ti-3 Al-2.5 V Applications: Exhaust systems, bicycle frames, eye glass frames.Features:High strength, excellent balance between strength and toughness.Information provided by K.. |
|||
Tensile Strength, Ultimate | 620 - 870 MPa | 89900 - 126000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 620 - 900 MPa | 89900 - 131000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 620 - 900 MPa | 89900 - 131000 psi | |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 620 - 800 MPa | 89900 - 116000 psi | |
Materion Beryllium Copper Alloy 25 Wire; 1/4H (TD01) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 620 - 900 MPa | 89900 - 131000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | >= 620 MPa | >= 89900 psi | |
MetalTek MTEK 175-B Cast UNS C95410 Aluminum Bronze Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov.. |
|||
Tensile Strength, Ultimate | >= 620 MPa | >= 89900 psi | |
MetalTek MTEK 175-C Cast UNS C95400HT Aluminum Bronze Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov.. |
|||
Tensile Strength, Ultimate | >= 620 MPa | >= 89900 psi | |
MetalTek MTEK 2205 Cast UNS J92205 Duplex Stainless Steel Excellent seawater corrosion resistance combined with nearly twice the strength of common stainless steels.Applications: Offshore piping systems, couplings. Centrifuge, dewatering equipment. Pump, v.. |
|||
Tensile Strength, Ultimate | >= 620 MPa | >= 89900 psi | |
MetalTek Nitronic® 40 Austenitic Stainless Steel Produced under license of ARMCO Advanced Materials Corp. Information provided by MetalTek |
|||
Tensile Strength, Ultimate | 620 MPa | 89900 psi | |
Haynes Hastelloy® W alloy as a weld filler, base metal Type 304 Stainless steel 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Tensile Strength, Ultimate | 620 - 870 MPa | 89900 - 126000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 620 MPa @Temperature 760 °C |
89900 psi @Temperature 1400 °F |
|
Haynes 188 alloy, cold rolled and 1175°C solution annealed sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Ultimate | 620 MPa @Temperature 550 °C |
89900 psi @Temperature 1020 °F |
Annealed prior to test |
Special Metals INCONEL® Alloy C-276 A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially .. |
|||
Tensile Strength, Ultimate | 620 MPa | 89900 psi | |
SSAB Tunnplat Domex® 044 BOR Rolled Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Ultimate | >= 620 MPa | >= 89900 psi | |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Annealed Cold Workable Medium Strength Alloy. UTS, TYS, Elongation, R.A. and bend radius data below are specific to annealed material; other specific condition entries are also available in MatWeb.Features.. |
|||
Tensile Strength, Ultimate | 620 MPa | 89900 psi | Typical |
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); Annealed Cold Formable Medium-Strength AlloyIndustry Specifications: Germany Aerospace: 3.7124. France: T-U2. UK Aerospace Specifications BA TA. 21, 22, 23.Features: This binary, age hardening alloy combi.. |
|||
Tensile Strength, Ultimate | 620 - 720 MPa | 89900 - 104000 psi | |
CLAL-MSX NICLAFOR® 1000 TD3 Quenched/Cold Rolled, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Tensile Strength, Ultimate | 620 MPa | 89900 psi | |
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |
|||
Tensile Strength, Ultimate | 620 MPa | 89900 psi | |
Carpenter HyMu "80"® Electronic Alloy, Bar, After Process Anneal Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Tensile Strength, Ultimate | 620 MPa | 89900 psi | Solution Treated (Typical) |
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286 Allegheny Ludlum Altemp A286 alloy is an iron-base superalloy useful for applications requiring high strength and corrosion resistance up to 704 degrees Celsius and for lower stress applications at .. |
|||
Tensile Strength, Ultimate | 620 MPa | 89900 psi | |
ATI Allegheny Ludlum Grade 12 Titanium (UNS R53400) Uses: heat exchangers, industrial components, tubing, CPI equipment.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Ultimate | 620 MPa | 89900 psi | ASTM D638 |
Quantum Composites QC-8805 66% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8805 is a vinyl ester-based sheet molding compound (SMC) reinforced with continuous, unidirectional (0°) glass fibers. It provides high strength, stiffness, and fatigue resistance in the fiber .. |
|||
Tensile Strength, Ultimate | 620 MPa | 89900 psi | Annealed prior to test |
Special Metals INCOLOY® Alloy 020 A nickel-iron-chromium alloy with additions of copper and molybdenum. It also contains niobium for stabilization against sensitization and resultant intergranular corrosion. The alloy has excellen.. |