Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 441 MPa | 64000 psi | Typical |
PSM Industries PolyAlloys MIM-4605 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | 441 MPa | 64000 psi | Annealed |
Special Metals MONEL® Alloy 401 A copper-nickel alloy designed for specialized electrical and electronic applications. It has a very low temperature coefficient of resistance and medium-range electrical resistivity. Used for wir.. |
|||
Tensile Strength, Ultimate | 441 - 490 MPa | 64000 - 71000 psi | |
Eagle Brass 151 ZHC® COPPER, Spring Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Ultimate | >= 441 MPa | >= 64000 psi | |
Eagle Brass 19210 XP-10 Copper Iron, Spring 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Strength, Ultimate | 441 - 496 MPa | 64000 - 72000 psi | |
Eagle Brass 220 Commercial Bronze, Extra Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Strength, Ultimate | 441 - 510 MPa | 64000 - 74000 psi | |
Eagle Brass 260 Cartridge Brass, 3/4 Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Tensile Strength, Ultimate | 441 MPa @Temperature 538 °C |
64000 psi @Temperature 1000 °F |
|
AK Steel 309S Austenitic Stainless steel AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic w.. |
|||
Tensile Strength, Ultimate | 441 MPa | 64000 psi | |
Ametek P409L P/M Stainless Steel, Sintered from 6.60 g/cc Green Density P409L is a ferritic, weldable grade of stainless steel with high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance and ha.. |
|||
Tensile Strength, Ultimate | 441 MPa @Temperature 93.3 °C |
64000 psi @Temperature 200 °F |
200°F |
ATI Allegheny Ludlum Stainless Steel Type AL 436S™ Ferric Stainless Steel The AL 436S™ alloy has a body-centered cubic, ferritic microstructure at all temperatures below the melting point. Angular titanium carbo-nitiride particles occur randomly in the ferrite matrix mi.. |
|||
Tensile Strength, Ultimate | 441 MPa @Temperature 538 °C |
64000 psi @Temperature 1000 °F |
|
AK Steel 309 Austenitic Stainless steel AK Steel 309 provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic wh.. |
|||
Tensile Strength, Ultimate | 441 MPa | 64000 psi | |
Ametek P409L/409CB P/M Stainless Steel, Sintered from 6.60 g/cc Green Density P409L/409CB is a ferritic, weldable grade of stainless steel with high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance .. |
|||
Tensile Strength, Ultimate | 441 - 517 MPa | 64000 - 75000 psi | |
AK Steel 436L ULTRA FORM® Ferritic Stainless Steel AK Steel’s 436L ULTRA FORM® is a ferritic grade of stainless steel that outperforms Type 409 in oxidation resistance and corrosion testing. The addition of molybdenum enhances pitting resistance w.. |