Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 483 MPa | 70000 psi | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70100 psi | |
Hogen Duralloy H5TC 50 Tungsten Carbide/50 Copper PM Metal Composite Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Used for light duty projection weld.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70100 psi | |
Hogen H20S, 26 Silver/74 Tungsten PM Metal Composite RWMA Class EDMDURAKUT Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Chemica.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70000 psi | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Tensile Strength, Ultimate | 483 MPa @Temperature 760 °C |
70100 psi @Temperature 1400 °F |
|
Kennametal Stellite Deloro® 208 PM after P/M Processing Adhesive wear test data: cast 0.06 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, s.. |
|||
Tensile Strength, Ultimate | 483 MPa @Temperature 649 °C |
70100 psi @Temperature 1200 °F |
|
Kennametal Stellite Stellite® 3 PM cast Typical applications include (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) diesel engine exhaust, fluid valve seats, saw cutt.. |
|||
Tensile Strength, Ultimate | 483 MPa @Temperature 760 °C |
70100 psi @Temperature 1400 °F |
|
Kennametal Stellite Stellite® 3 PM cast Typical applications include (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) diesel engine exhaust, fluid valve seats, saw cutt.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70000 psi | |
Kinetics MIM 2.5% SiFe Soft Magnetic Steel Low alloy steel, silicon. A work hardenable steel alloy that offers very good magnetic properties, tensile strength, hardness, wear resistance, and increased spring steel strength. Can be plated or .. |
|||
Tensile Strength, Ultimate | 483 MPa | 70000 psi | |
FloMet Fe-3% Si Soft Magnetic Alloy FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |
|||
Tensile Strength, Ultimate | 483 - 517 MPa | 70000 - 75000 psi | |
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70100 psi | |
Mi-Tech Metals SW74 26 Silver/74 Tungsten PM Metal Composite RWMA Class EDMMi-Tech Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Chemica.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70000 psi | |
Universal Wire Works 190 Nickel Alloy Welding Wire Alloy 190 is used for arc welding Monel type alloys 400 and 404 to themselves or to one another, as well as overlaying on steel. Typical applications include welding ASTM B127, B163, B164, and B165... |
|||
Tensile Strength, Ultimate | 483 MPa | 70000 psi | |
Universal Wire Works 60 Nickel Alloy Welding Wire Alloy 60 is used for Gas Metal Arc Welding (GMAW), Gas Tungsten Arc Welding (GTAW), and Submerged Arc Welding (SMA) of Monel type alloys 400 and 404, as well as overlaying on steel. When GMAW or MIG.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70000 psi | |
Universal Wire Works No. 1 Cobalt Alloy Welding Wire Universal No. 1 is a cobalt-chromium-tungsten alloy suited for applications requiring extreme abrasion resistance at elevated temperatures. Excellent for resistance to corrosion and oxidation where .. |
|||
Tensile Strength, Ultimate | 483 - 565 MPa | 70000 - 82000 psi | |
Eagle Brass 425 Tin Brass 2%, Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70000 psi | 18-20in thickness |
Clinton Aluminum Alumold 1-500 Forged Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is .. |
|||
Tensile Strength, Ultimate | 483 MPa | 70000 psi | annealed |
CMW® ELKONIUM 34 platinum based alloy Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70000 psi | annealed |
CMW® ELKONIUM 405 palladium based alloy Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70100 psi | |
AK Steel 430 Ferritic Stainless steel AK Steel 430 combines good corrosion resistance and heat and oxidation resistance up to 1500°F with good mechanical properties. Typical consumer applications include automotive trim and molding, f.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70000 psi | Semi-Processed |
AK Steel DI-MAX® M-43 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Tensile Strength, Ultimate | 483 - 621 MPa | 70100 - 90100 psi | |
Ametek High Purity Nickel Strip 899A 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 483 - 621 MPa | 70100 - 90100 psi | |
Ametek High Purity Nickel Strip 899L 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 483 MPa @Temperature 538 °C |
70100 psi @Temperature 1000 °F |
ASTM E8 |
ATI Allegheny Ludlum 310 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | >= 483 MPa | >= 70100 psi | Annealed |
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |
|||
Tensile Strength, Ultimate | 483 MPa | 70100 psi | |
ATI Allvac® Grade 12 UNS R53400 Titanium Alloy Uses: Industrial components. CPI equipment, heat exchangers, pressure vessels, fittings, tubing.Property values are for samples in the metallurgical condition: 1300°F anneal.Information provided by.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70000 psi | 90° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70000 psi | 0° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Tensile Strength, Ultimate | 483 MPa | 70100 psi | |
ATI Allegheny Ludlum Grade 7 Titanium (UNS R52400) Uses: CPI equipment, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |