Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 434 - 496 MPa | 63000 - 72000 psi | |
Eagle Brass 230 Red Brass, Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Ultimate | 434 - 517 MPa | 63000 - 75000 psi | |
Eagle Brass 521 Phosphor Bronzes 8% C, 1/4 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Ultimate | 434 - 517 MPa | 63000 - 75000 psi | |
Eagle Brass 735 Nickel Silver 18%, 1/2 Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 434 MPa | 62900 psi | 5% Cold Worked |
AK Steel 409 ULTRA FORM® Stainless Steel AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and .. |
|||
Tensile Strength, Ultimate | 434 MPa | 63000 psi | |
AK Steel DI-MAX® M-36 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Tensile Strength, Ultimate | 434 MPa | 62900 psi | typical annealed |
ATI Allegheny Ludlum AL 409HP™ Ferritic Stainless Steel, UNS S40930 Type 409 ferritic stainless steel was introduced by Allegheny Ludlum in 1961 to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon automotive .. |