Polymer Property : Tensile Strength, Ultimate = 5400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.7 - 37.3 MPa
1990 - 5400 psi
ASTM D638
Polikim EFALON® T-100 Virgin PTFE
Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu..
Tensile Strength, Ultimate 31.0 - 37.2 MPa
4500 - 5400 psi
Polypropylene; ASTM D638M
DSM Somos® 9120
The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp..
Tensile Strength, Ultimate 12.0 - 37.2 MPa
1740 - 5400 psi
Average value: 25.7 MPa Grade Count:47
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..