BCC Products BC 7136 Epoxy Casting

Category Polymer , Thermoset , Epoxy
Manufacturer BCC Products
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 7136 Epoxy Casting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC7136 is a gray, low toxicity, aluminum filled, epoxy casting resin. This heat resistant system may be used at room temperature without post-curing. May be cast to a thickness of ¾ inch in non-conductive molds. For use above 150ºF a post-cure is required. This product was engineered to replace VCHD and MDA systems while retaining excellent heat resistance and low viscosity. BC7136 is designed for consistent use up to 300ºF. Uses: heat resistant tooling, constructing vacuum form tools, injection and compression molds, RTM and RIM molds, matched dies.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.69 g/cc
1.69 g/cc
Brookfield Viscosity 15000 cP

@Temperature 23.9 °C
15000 cP

@Temperature 75.0 °F
Mixed
Linear Mold Shrinkage 0.0011 cm/cm
0.0011 in/in
ASTM D2566-69
Mechanical Properties Metric English Comments
Hardness, Shore D 90

@Temperature 23.9 °C
90

@Temperature 75.0 °F
Tensile Strength, Ultimate 53.8 MPa
7800 psi
Flexural Strength 59.3 MPa
8600 psi
Compressive Strength 200 MPa
29000 psi
Thermal Properties Metric English Comments
CTE, linear 34.2 µm/m-°C
19.0 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 152 °C
305 °F
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 24.0 °C
24.0 hour

@Temperature 75.2 °F
Pot Life 85 min

@Temperature 24.0 °C
85 min

@Temperature 75.2 °F
1 lb. mass
Descriptive Properties Value Comments
Mix Ratio 100:7 by weight, 100:12 by volume, resin/harder