Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CPC - Vycom SEABOARD™ GRIP-X™ Slip Resistant High Density Polyethylene (HDPE)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer CPC - Vycom Co.
Trade Name SEABOARD™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CPC - Vycom SEABOARD™ GRIP-X™ Slip Resistant High Density Polyethylene (HDPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grip-X is a UV stabilized high density polyethylene (HDPE) sheet formulated to meet demanding conditions of the marine industry. Grip-X is manufactured with a special surface treatment and stipulated pattern to achieve a slip resistant surface as compared with the standard surface and other high density polyethylene marine grade products.FEATURES AND BENEFITS Stability- Grip-X is UV stabilized to endure the test of time outdoors. Strength- Grip-X is made from the same strong polymer base as Seaboard, simply the toughest material available. Inert- Grip-X is impervious to salt and moisture in marine environments. Surface- Grip-X has a unique elastomer surface that provides additional traction in both wet and dry conditions. Consistency- Grip-X is extruded for the most dimensional consistency.Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 25 hour
25 hour
F50; ASTM D1693
>= 500 hour
>= 500 hour
F50; ASTM D2561
Melt Index of Compound 0.70 g/10 min
0.70 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ASTM D2240
Tensile Strength, Ultimate 30.3 MPa
4400 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Tensile Impact 53.4 J/cm
100 ft-lb/in
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C
172 °F
ASTM D648
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Brittleness Temperature <= -7.78 °C
<= 18.0 °F
ASTM D746