Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BCC Products EB 6200 Epoxy Tooling Board

Category Polymer , Thermoset , Epoxy , Epoxy Molding Compound
Manufacturer BCC Products
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products EB 6200 Epoxy Tooling Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EB6200 is a “grain-free” elevated temperature epoxy modeling material known for its superior surface finish, dimensional stability and the ability to maintain tolerances even after being subjected to temperature variations. EB6200 has excellent dimensional stability results from the low coefficient of thermal expansion and high glass transition temperature. Applications: Master Models (Aerospace); Automotive Die Models; Vacuum Forming at Elevated Temperatures; Lay-Up Tools for Medium and High Temperature Curing PrepregInformation provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.760 g/cc
0.760 g/cc
ASTM-D-792-66
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ASTM D2240
Tensile Strength, Ultimate 30.3 MPa
4400 psi
ASTM D638
Flexural Strength 35.5 MPa
5150 psi
ASTM D790
Flexural Modulus 2.41 GPa
349 ksi
ASTM-D-790
Compressive Strength 33.1 MPa
4800 psi
ASTM D695
Compressive Modulus 2.36 GPa
342 ksi
ASTM-D-695
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Izod Impact Unnotched 1.42 J
1.05 ft-lb
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 37.8 µm/m-°C
21.0 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 149 °C
300 °F
ASTM-D-648-56
Glass Transition Temp, Tg >= 163 °C
>= 325 °F
ASTM D3418
Copyright © lookpolymers.com All Rights Reserved