Abatron AboCast 8103-11 One Part Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Abatron
Trade Name AboCast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8103-11 One Part Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One component system. Information provided by Abatron, Inc.Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 190 min. at 100°C (212°C). Peak exotherm 170°C (340°F). At 100°C (212°F), gels in 3-4 hrs, total cure in 4-6 hrs. At 110-120°C (230-250°F) gels to 0.5-1 hr and total cure in 1-2 hrs.
Physical Properties Metric English Comments
Viscosity Measurement 12000
12000
Mechanical Properties Metric English Comments
Hardness, Rockwell M 111
111
Tensile Strength, Ultimate 39.0 MPa
5660 psi
Elongation at Break 1.6 %
1.6 %
Flexural Yield Strength 96.53 MPa
14000 psi
Flexural Modulus 3.10 GPa
450 ksi
Compressive Yield Strength 113.8 MPa
16510 psi
Compressive Modulus 2.28 GPa
330 ksi
2.30 GPa
334 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 9.63e+15 ohm-cm
9.63e+15 ohm-cm
Surface Resistance 7.85e+15 ohm
7.85e+15 ohm
Dielectric Constant 3.15

@Frequency 1e+6 Hz
3.15

@Frequency 1e+6 Hz
3.35

@Frequency 1000 Hz
3.35

@Frequency 1000 Hz
3.36

@Frequency 60 Hz
3.36

@Frequency 60 Hz
Dissipation Factor 0.0035

@Frequency 60 Hz
0.0035

@Frequency 60 Hz
0.055

@Frequency 1000 Hz
0.055

@Frequency 1000 Hz
0.23

@Frequency 1e+6 Hz
0.23

@Frequency 1e+6 Hz
Descriptive Properties Value Comments
Exotherm 170°C
Peak