Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer BASF
Trade Name Elastollan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fuel and solvent resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing.Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D412
Tensile Strength, Yield 1.30 MPa

@Strain 300 %
189 psi

@Strain 300 %
ASTM D-412
6.60 MPa

@Strain 100 %
957 psi

@Strain 100 %
ASTM D-412
Elongation at Break 620 %
620 %
ASTM D412
Modulus of Elasticity 0.0200 GPa
2.90 ksi
Shear Modulus 0.0120 GPa
1.74 ksi
Tear Strength 95.0 kN/m
542 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 25
25
H-18 wheel; ASTM D-1044.
Tensile Set 35 %
35 %
at break; ASTM D-412
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
Flammability, UL94 HB

@Thickness 0.950 mm
HB

@Thickness 0.0374 in
Color: NC.
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V
>= 600 V
DIN/IRC 112