Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.0 - 160 MPa

@Temperature -50.0 - 250 °C
6530 - 23200 psi

@Temperature -58.0 - 482 °F
Average value: 101 MPa Grade Count:1
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Tensile Strength, Ultimate 34.5 - 160 MPa
5000 - 23200 psi
Average value: 75.2 MPa Grade Count:26
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Tensile Strength, Ultimate 88.0 - 160 MPa
12800 - 23200 psi
Average value: 124 MPa Grade Count:14
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Tensile Strength, Ultimate 0.414 - 160 MPa
60.0 - 23200 psi
Average value: 7.11 MPa Grade Count:508
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Tensile Strength, Ultimate 100 - 160 MPa

@Temperature 60.0 - 150 °C
14500 - 23200 psi

@Temperature 140 - 302 °F
Average value: 131 MPa Grade Count:1
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Tensile Strength, Ultimate 26.2 - 160 MPa
3800 - 23200 psi
Average value: 121 MPa Grade Count:41
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..
Tensile Strength, Ultimate 40.0 - 160 MPa

@Strain 1.00 - 9.00 %
5800 - 23200 psi

@Strain 1.00 - 9.00 %
Average value: 104 MPa Grade Count:1
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Tensile Strength, Ultimate 40.0 - 160 MPa

@Temperature 60.0 - 150 °C
5800 - 23200 psi

@Temperature 140 - 302 °F
Average value: 104 MPa Grade Count:1
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Tensile Strength, Ultimate 150 - 160 MPa

@Temperature 80.0 - 80.0 °C
21800 - 23200 psi

@Temperature 176 - 176 °F
Average value: 155 MPa Grade Count:2
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Tensile Strength, Ultimate 30.0 - 160 MPa

@Temperature -40.0 - 150 °C
4350 - 23200 psi

@Temperature -40.0 - 302 °F
Average value: 66.6 MPa Grade Count:7
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Tensile Strength, Ultimate 44.8 - 160 MPa
6500 - 23200 psi
Average value: 87.1 MPa Grade Count:21
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..