Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 41.4 - 95.0 MPa | 6000 - 13800 psi | Average value: 75.7 MPa Grade Count:19 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Tensile Strength, Ultimate | 10.0 - 95.0 MPa @Temperature -20.0 - 100 °C |
1450 - 13800 psi @Temperature -4.00 - 212 °F |
Average value: 49.1 MPa Grade Count:1 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Tensile Strength, Ultimate | 10.0 - 95.0 MPa @Strain 1.00 - 3.00 % |
1450 - 13800 psi @Strain 1.00 - 3.00 % |
Average value: 49.1 MPa Grade Count:1 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Tensile Strength, Ultimate | 35.0 - 95.0 MPa @Temperature 60.0 - 150 °C |
5080 - 13800 psi @Temperature 140 - 302 °F |
Average value: 58.8 MPa Grade Count:2 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Tensile Strength, Ultimate | 85.0 - 95.0 MPa | 12300 - 13800 psi | Typical |
ATI Allegheny Ludlum AL 20™ Plate Specialty Steel The N08020 alloy has been available for many years and has found applications in many environments, such as in chlorides and in sulfuric and sulfurous acids.Although AL 20 alloy was developed for im.. |
|||
Tensile Strength, Ultimate | 70.0 - 95.0 MPa @Temperature 60.0 - 150 °C |
10200 - 13800 psi @Temperature 140 - 302 °F |
Average value: 82.5 MPa Grade Count:1 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |