Polymer Property : Tensile Strength, Ultimate = 125 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.73 - 125 MPa

@Temperature -40.0 - 160 °C
541 - 18100 psi

@Temperature -40.0 - 320 °F
Average value: 53.1 MPa Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Tensile Strength, Ultimate 3.73 - 125 MPa

@Strain 0.250 - 10.0 %
541 - 18100 psi

@Strain 0.250 - 10.0 %
Average value: 53.1 MPa Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Tensile Strength, Ultimate 97.0 - 125 MPa
14100 - 18100 psi
Average value: 113 MPa Grade Count:15
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Tensile Strength, Ultimate 50.0 - 125 MPa

@Temperature 0.000 - 160 °C
7250 - 18100 psi

@Temperature 32.0 - 320 °F
Average value: 67.6 MPa Grade Count:4
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Tensile Strength, Ultimate 50.0 - 125 MPa
7250 - 18100 psi
Average value: 90.5 MPa Grade Count:6
Overview of materials for Phenolic, Resole, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Tensile Strength, Ultimate 110 - 125 MPa

@Temperature 130 - 175 °C
16000 - 18100 psi

@Temperature 266 - 347 °F
Average value: 128 MPa Grade Count:4
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Tensile Strength, Ultimate 110 - 125 MPa

@Time 1.80e+7 - 7.20e+7 sec
16000 - 18100 psi

@Time 5000 - 20000 hour
Average value: 128 MPa Grade Count:4
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Tensile Strength, Ultimate 89.6 - 125 MPa
13000 - 18100 psi
Average value: 100 MPa Grade Count:8
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are ..
Tensile Strength, Ultimate 52.0 - 125 MPa

@Temperature 0.000 - 160 °C
7540 - 18100 psi

@Temperature 32.0 - 320 °F
Average value: 78.5 MPa Grade Count:2
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..