Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP FARADEX WX94736 PBT LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RCL26 PA6.6 LNP* LUBRICOMP* RCL26 is a compound based on Nylon 66 containing 30% Carbon Fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Electrically Conductive. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 LNP LUBRICOMP* RP004 is a compound based on Nylon 66 resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 (Asia Pacific) LNP* Lubricomp* RP004 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXP PPA LNP LUBRICOMP* UFL36SXP is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP UX96507 PPA LNP* LUBRICOMP* UX96507 is a compound based on PPA containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP WL002 PBT LNP* LUBRICOMP WL002 is a compound based on PBT resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP ZFG26 PPE+PS (Asia Pacific) LNP* Lubricomp* ZFG26 is a compound based on PPE+PS Blend resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM UC1200 PEI (Asia Pacific) 12% carbon fiber reinforced Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 listing in recognized colors. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® IQNH4550 PBT Valox* iQNH4550 resin is a glass filled, non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% .. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON RX05488 PA 66 LNP STAT-KON* RX05488 is a compound based on Nylon 66 resin containing Carbon Fiber, Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS LNP THERMOCOMP* AH0230A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP EC006E PEI LNP THERMOCOMP* EC006E is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF006 PA 66 LNP* THERMOCOMP* RF006 is a compound based on Nylon 66 resin containing 30% Glass Fiber. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF006H PA 66 LNP THERMOCOMP* RF006H is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXH PA 66 LNP* THERMOCOMP* RF006XXH is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF007ES PA 66 LNP* THERMOCOMP* RF007ES is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Easy Molding. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP YF002 POLYESTER ELASTOMER LNP* THERMOCOMP* YF002 is a compound based on Poyester Elastomer containing 10% Glass Fiber. Added feature of this grade is: High Modulus. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 6 |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66 LNP* LUBRICOMP* RI001 is a compound based on Nylon 66 resin containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Dart Drop, Total Energy | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly (Asia Pacific) LNP* Thermocomp* KFB11 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP QCP36 PA 6/10 (Asia Pacific) LNP* Lubricomp* QCP36 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conducti.. |
|||
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP JF006EXZ PES LNP* THERMOCOMP* JF006EXZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |